GSO ISO 34-1:2015

ISO 34-1:2010
Gulf Standard   Current Edition · Approved on 03 September 2015

Rubber, vulcanized or thermoplastic -- Determination of tear strength -- Part 1: Trouser, angle and crescent test pieces

GSO ISO 34-1:2015 Files

English 13 Pages
Current Edition Reference Language
29.85 BHD

GSO ISO 34-1:2015 Scope

This part of ISO 34 specifies three test methods for the determination of the tear strength of vulcanized or thermoplastic rubber, namely: — method A, using a trouser test piece; — method B, using an angle test piece, with or without a nick of specified depth; — method C, using a crescent test piece with a nick. The value of tear strength obtained depends on the shape of the test piece, speed of stretching, and temperature of test. It can also be susceptible to grain effects in rubber. Method A: Using a trouser test piece Method A, using the trouser test piece, is preferred because it is not sensitive to the length of the cut, unlike the other two test pieces in which the nick has to be very closely controlled. In addition, the results obtained are more easily related to the fundamental tear properties of the material and are less sensitive to modulus effects (provided that the leg extension is negligible) and the rate of propagation of the tear is directly related to the rate of grip separation. With some rubbers, the propagation of tear is not smooth (knotty tear), and analysis of results can be difficult[3]. Method B, procedure (a): Using an angle test piece without nick This test is a combination of tear initiation and propagation. Stress is built up at the point of the angle until it is sufficient to initiate a tear and then further stresses propagate this tear. However, it is only possible to measure the overall force required to rupture the test piece, and, therefore, the force cannot be resolved in two components producing initiation and propagation[4]. Method B, procedure (b): Using an angle test piece with nick This test measures the force required to propagate a nick already produced in the test piece. The rate of propagation is not directly related to the jaw speed[5]. Method C: Using a crescent test piece This test also measures the force required to propagate a nick already produced in the test piece, and the rate of propagation is not related to the jaw speed. NOTE A separate method for the determination of the tear strength of small test pieces of rubber (Delft test pieces) is specified in ISO 34-2[1].

Best Sellers From Chemical and Textile Sector

GSO 1943:2024
 
Gulf Technical Regulation
Cosmetic Products – Safety Requirements of Cosmetics and Personal Care Products
BH GSO 1943:2024
GSO 1943:2024 
Bahraini Technical Regulation
Cosmetic Products – Safety Requirements of Cosmetics and Personal Care Products
GSO 151:2022
 
Gulf Standard
Synthetic Detergents –Household Synthetic Detergents Powder
BH GSO 151:2023
GSO 151:2022 
Bahraini Standard
Synthetic Detergents –Household Synthetic Detergents Powder

Recently Published from Chemical and Textile Sector

GSO 276:2003
 
Gulf Standard
METHODS OF TESTING OF HEAD CLOTH FOR MEN — COTTON SHEMAGH AND POLYESTER SHEMAGH BLENDED OR COTTON SYNTHETIC FIBRES SHEMAGH
GSO 226:2003
 
Gulf Standard
METHODS OF TEST FOR HEAD CLOTH FOR MEN — WHITE GHAUTRA
GSO 1135:2002
 
Gulf Standard
DETERMINATION OF FREE SULPHUR IN FERTILIZERS
GSO ISO 672:1994
ISO 672:1978 
Gulf Standard
Soaps - Determination of moisture and volatile matter content - Oven method .